Pouring of moulds

 

The melted iron is taken from the furnace into the ladle from which it is poured into the moulds in the casting area. The pouring temperature is about 1,320 – 1,440°C. The shake-out of moulds takes place 8 – 60 hours after pouring, depending on the size and material of the casting.